Re: peroxide compatibility question

[email protected]
Newsgroups gmane.technology.erps
Message-ID <[email protected]>
PCB's are typically HASL coated (hot air solder level) and not pure tin.   
Its just that
many platings are noncontinuous and have pinholes, which could cause flaking. 
  A pure
tin coating may work fine, I just can't say for sure.

Dan

In a message dated 3/28/04 8:32:23 PM, [email protected] writes:


> Tin sure sticks to the copper of PC boards.
> 
> --- [email protected] wrote:
> > . . . I don't know if Tin would be adherent
> > enough for this purpose.
> >
>